聚己内酯型高耐温级,具有很高的机械强度、优异的耐磨性、压缩变形率、可承受较大动态载荷。适合于高性能注塑产品,如密封件和辊轮。
品名 Product Code No. |
|
|
KT90A |
KT95A |
物性 Properties |
测试方法 Method |
单位 |
|
|
硬度 Hardness |
ASTM |
Shore A |
90±2 |
95±2 |
|
ASTM |
Shore D |
|
|
比重 Specific Gravity |
ASTM |
|
1.18 |
1.19 |
拉伸强度Tensile strength |
ASTM |
Kg/cm2 |
490 |
505 |
伸长率 Elongation |
ASTM |
% |
530 |
490 |
100%模量 100%Modulus |
ASTM |
Kg/cm2 |
75 |
105 |
磨耗性 Abrasion |
ASTM |
mm3 |
20 |
20 |
撕裂强度 Tear Strength |
ASTM |
Kg/cm2 |
11 |
13 |
压缩变形率24h@23℃ |
ASTM |
% |
13 |
14 |
压缩变形率70h@100℃ |
ASTM |
% |
34 |
38 |
建议加工温度 Processing temp |
|
℃ |
195-210 |
200-215 |
注 意: |